CN-8760G A/B
|
Property |
Unit |
Value |
|
Viscosity (Mixed) |
cP |
3200 |
|
mPa-sec |
3200 |
|
|
Pa-sec |
3.2 |
|
|
Specific Gravity (Cured) |
- |
1.58 |
|
Working Time @ 25C (Pot Life - minutes) |
minutes |
100 |
|
Cure Time at 25ºC |
hrs |
24 |
|
Cure Time @ 60ºC |
minutes |
30 |
|
Durometer Shore A |
- |
45 |
|
Tensile Strength |
psi |
265 |
|
MPa |
1.8 |
|
|
kg/cm2 |
18 |
|
|
Elongation |
% |
85 |
|
Thermal Conductivity |
btu/hr ft degF |
0.387 |
|
W/mK |
0.67 |
|
|
Dielectric Strength |
volts/mil |
625 |
|
kV/mm |
24 |
|
|
Dielectric Constant at 100 Hz |
- |
2.88 |
|
Dielectric Constant at 100 kHz |
- |
2.66 |
|
Dissipation Factor at 100 hz |
- |
0.03 |
|
Dissipation Factor at 100 kHz |
- |
0.06 |
|
Volume Resistivity ohm*cm |
ohm*cm |
1.00E+17 |
|
UL Flammability Classification |
NA |
94 V-0 |
|
Shelf Life at 25ºC |
months |
9 |
FEATURES
• Low viscosity
• Good thermal conductivity
• Good reworkability
• Non-corrosive to metal
• 1:1 mixing ratio
• Room temperature curing